AMC VLA 613(c) Material strength properties and design values
(Acceptable Means of Compliance)
ED Decision 2003/18/RM
Test Temperature -
a. For white painted surface and vertical sunlight: 54°C. If the test cannot be performed at this temperature an additional factor of 1.25 should be used.
b. For other coloured surfaces the curve below may be used to determine the test temperature.
Curve based on: NASA Conference Publication 2036
NASA Contractor Report 3290